After more than ten years of exploration and accumulation, we have solved the demanding requirements of brand customers for excellent electroplating quality. Customize customer-specific electroplating color, thickness of electroplating layer, color retention time, etc. Flash plating for brass and silver materials , PVD plating for stainless steel materials .

S&J Advanced Waterproof Plating Technology

S&J provides two different surface-finishing systems for jewelry brands: vacuum-ion PVD coating for stainless steel, and wet electroplating for brass and silver. The appropriate solution depends on the base metal, design, target color, intended use, order volume and required testing standard.

Our regular production specification for both PVD coating and electroplating is 0.03–0.08 μm. For selected brass or silver jewelry projects, custom heavy electroplating from 1.0–2.5 μm can also be developed when the product specification and commercial requirements justify the additional deposit.

Choose the Right Plating System for Your Jewelry

Similar thickness values do not mean the same manufacturing process or the same coating performance. The correct solution starts with the base metal and intended application.

PVD Coating for Stainless Steel

For 316L stainless steel jewelry, S&J uses a 0.03–0.08 μm vacuum-ion PVD coating as the regular production specification. This thin, dense coating supports strong adhesion, water resistance and long-term color performance when surface preparation and process control are properly managed.

  • 316L stainless steel
  • Standard thickness: 0.03–0.08 μm
  • Vacuum-ion deposition
  • Suitable for waterproof and daily-wear jewelry

Explore PVD Coating →

Electroplating for Brass and Silver

For brass and silver jewelry, S&J’s regular wet-electroplating specification is also 0.03–0.08 μm. Selected projects may require 1.0–2.5 μm heavy electroplating when a thicker precious-metal deposit forms part of the approved product specification.

  • Brass and silver base metals
  • Standard thickness: 0.03–0.08 μm
  • Custom heavy plating: 1.0–2.5 μm
  • Subject to design, MOQ and target cost

Important: Coating thickness is only one quality variable. PVD performance also depends on coating density, adhesion, substrate stability, surface preparation and controlled vacuum deposition; electroplating performance depends on the base metal, plating sequence, deposit composition, protective coating and final quality control.

Wet Electroplating Process for Brass and Silver

The steps below describe S&J’s wet-electroplating workflow for brass and silver jewelry. Stainless steel PVD follows a separate vacuum-ion-deposition process and should not be interpreted through the same production sequence. Explore S&J’s PVD coating solution.

High density precision polishing

Our experienced craftsmen patiently polish the brass and silver chain links before immersing them in an electrolytic bath that is composed of a solution of salts, including the metal to be plated.

Display before process

Anodic Clean

Sulphuric Acid Etching

Electro Plating

High temperature or low temperature treatment

High density precision polishing

Display before process

Anodic Clean

Sulphuric Acid Etching

Electro Plating

High temperature or low temperature treatment

Professional Tests for Plating Quality

Neutral Salt Spray Test

Key steps:

Spray salt water containing (5±0.5)% sodium chloride with a pH value of 6.5 to 7.2 through a spray device, let the salt spray settle on the test piece to be tested, and observe its surface Corrosion state after a certain period of time (24 hours to 72 hours).

The temperature of the test box is required to be (35±2)℃, the humidity is greater than 95%, the amount of mist reduction is 1 to 2 mL/(h·cm2), and the nozzle pressure is 78.5 to 137.3kPa (0.8 to 1.4kgf/cm2).

When the test piece is placed in the box,do not directly contact the box body,but should be suspended or placed on a special shelf.

The sample holder is made of glass, plastic and other materials. The material for hanging the sample should not be metal, but rayon/cotton fiber or other insulating materials should be used.

Read Less Read More

Tumble Abrasion Test

Local Friction Test

Testing of Plating Hardness

Clamp the pencil in the instrument so that the pencil protrudes 5mm, and then place the instrument on the surface of the sample. Press the left key first, and the test platform moves to the left. The adjustment knob can be adjusted to the required test speed according to the test needs. The tachometer displays the motor speed in real time. Each time the motor rotates, the platform moves 1.75mm, and the sample to be tested is clamped On the test platform, click the right button, the test pencil slides on the sample plate at a certain speed, and it stops automatically when it reaches the end point.

Note : 1. Device is made in Germany.

2.Only standard 4H pencil used.

Plating Color Assessment Cabinet

Put the product in the box, press the button (UV key, D65 , etc.) to compare the color of the finished product under different lights to determine whether the finished product meets the requirements.

Note: International color standard applied in the system.

Testing of Plating Thickness

Note : Device is made in Germany .

Note : Device is made in Germany.

Thickness Measurement for Standard Coatings

Measurement range: below 1 μm. This equipment is used to verify standard jewelry coatings below 1 μm. S&J’s regular production specification for both stainless steel PVD coating and wet electroplating is 0.03–0.08 μm.

The equipment range describes measurement capability, not the default production thickness. Selected brass or silver projects may use 1.0–2.5 μm heavy electroplating when required by approved specifications.

Stainless steel PVD follows a separate vacuum-ion-deposition process from wet electroplating. Explore S&J’s PVD coating solution.